NR/SBR blends display an excellent resilience and good compression sets.
Standard Natural rubber, non staining
Basic elastomer : NR + SBR
Density in kg/m3 : 125 +/- 25
Compression -Deflection kPa (at 25%) : 35 -65
Factory : LEERS
Standard Natural rubber, non staining, firm grade
Basic elastomer : NR + SBR
Density in kg/m3 : 200 +/- 50
Compression -Deflection kPa (at 25%) : 50-85
Factory : LEERS
Excellent resilience and fatigue resistance, loss of resilience < 10% after 1 000 000 working cycles
Basic elastomer : NR + SBR
Density in kg/m3 : 220 +/- 25
Compression-Deflection kPa (at 25%) : 50-85
Factory : LEERS
Very firm product with good anti-vibrating properties
Basic elastomer : NR + SBR
Density in kg/m3 : 350 +/- 50
Compression-Deflection kPa (at 25%) : 120-220
Factory : AUREC
Extra firm product with good anti-vibrating properties
Basic elastomer : NR + SBR
Density in kg/m3 : 510 +/- 50
Compression-Deflection kPa (at 25%) : 200-500
Factory : AUREC