EPDM cellular rubbers have an excellent aging resistance, a good temperature resistance range and good compression sets.
EPDM standard grade with a good ageing resistance, no staining
Basic elastomer : EPDM
Density in kg/m3 : 130 +/- 20
Compression-Deflection kPa (at 25%) : 20-50
Factory : AUREC
Versatile EPDM, no staining
Basic elastomer : EPDM
Density in kg/m3 : 120 +/- 20
Compression-Deflection (at 25%) : 20-50
Factory : AUREC
Technical EPDM, good tear resistance, no staining
Basic elastomer : EPDM
Density in kg/m3 : 125 +/- 25
ompression
Deflection kPa (at 25%) : 35-65
Factory : AUREC
Optimized processing (thickness = 70 mm), no staining, versatile use
Basic elastomer : EPDM
Density in kg/m3 : 110 +/-25
Compression-Deflection kPa (at25%) : 20-50
Factory : AUREC
Excellent compression set , excellent ageing resistance
Basic elastomer : EPDM
Density in kg/m3 : 175 +/- 25
Compression-Deflection kPa (at 25%) : 35-65
Factory : AUREC
Excellent compression set, excellent weathering resistance
Basic elastomer : EPDM
Density in kg/m3 : 95 +/-25
Compression-Deflection kPa (at 25%) : 20-50
Factory : Leers
Technical EPDM, low compression set at high temperature, low fogging
Basic elastomer : EPDM
Density in kg/m3 : 175 +/- 25
Compression-Deflection kPa (at 25%) : 35-65
Factory : AUREC
Technical EPDM, excellent resistance at low temperature, excellent tightness after ageing
Basic elastomer : EPDM
Density in kg/m3 : 175 +/- 25
Compression-Deflection kPa (at 25%) : 35-65
Factory : AUREC
Technical EPDM, excellent resistance at high temperature
Basic elastomer : EPDM
Density in kg/m3 : 175 +/- 25
Compression-Deflection kPa (at 25%) : 35-65
Factory : AUREC
Soft EPDM SBR, good tear resistance
Basic elastomer : EPDM
SBR
Density in kg/m3 : 125 +/- 25
Compression-Deflection kPa (at 25%) : 15-35
Factory : LEERS
Very soft EPDM with closed cells, good thermal insulation
Basic elastomer : EPDM
Density in kg/m3 : 75 +/- 15
Compression-Deflection kPa (at 25%) : 12-28
Factory : AUREC
Very soft EPDM with closed cells, excellent resistance at high temperature
Basic elastomer : EPDM
Density in kg/m3 : 75 +/- 15
Compression-Deflection kPa (at 25%) : 12-28
Factory : AUREC
Soft EPDM for water and air sealing of irregular surfaces
(compression deflection ≥ 10 %). Excellent resistance to low and high temperatures
Basic elastomer : EPDM
Density in kg/m3 : 95 +/- 15
Compression-Deflection kPa (at 25%) : 0-15
Factory : LEERS
Zero sulfur – peroxide curing
EPDM for automotive and electronic applications, no staining, no corrosion on copper and silver
Basic elastomer : EPDM
Density in kg/m3 : 130 +/- 20
Compression-Deflection kPa (at 25%) : 35-65
Factory : AUREC
Zero sulfur – peroxide curing
EPDM for automotive and electronic applications, no staining, no corrosion on copper and silver
Basic elastomer : EPDM
Density in kg/m3 : 90 +/- 20
Compression-Deflection kPa (at 25%) : 20-50
Factory : Aurec